Product Parameter
ZHSU PPR antibacterial pipes are suitable for hot and cold potable water application, is a PPR pipe with double layer dense structure, inner anti-bacterial layer adopts high crystal nano-level active material,outer layer used food grade PPR raw material.
PPR antibacterial pipe is featured as light-blocking function,pipe is opaque, which makes the water inside the
pipe not easy to breed bacteria, prevented the microbial photosynthesis, prevent the pipe’s wall from moss growing, meanwhile characterized by high strength, low linear expansion coefficient and 50 years work time.
Our PPR antibacterial pipes’ outer layer are made of 100% new raw material from Borealis and South Korea , the inner anti-bacterial layer inside the pipe can release Ag ion which can kill bacteria inside the pipe, which ensures the health and safety of water or other fluids, makes the pipe highly hygienic and non-toxic
self-clean design keeps the pipe non-toxic and healthy from dirt accumulation
SPECIFICATIONS
Material : PPR raw material plus high crystal nano-level active material
Size : 20mm(1/2’’) to 160mm(6’’)
Pressure : PN10/S5 to PN20/S2.5
Color : Green, Purple and Grey for outer layer, milk white or transparent white for inner layer
Length : 4 meters, 3 meters, 5.8 meters per piece
Standard : ISO 15874,DIN 8077/8078, GB/T18742-2004
Connection : Socket fusion
Size (mm) | Size (inch) | PN10 | PN12.5 | PN16 | PN20 | ||||
Thickness (mm) | Weight (kg/meter) | Thickness (mm) | Weight (kg/meter) | Thickness (mm) | Weight (kg/meter) | Thickness (mm) | Weight (kg/meter) | ||
20 | 1/2'' | 2 | 0.114 | 2.3 | 0.127 | 2.8 | 0.148 | 3.4 | 0.172 |
25 | 3/4'' | 2.3 | 0.163 | 2.8 | 0.191 | 3.5 | 0.231 | 4.2 | 0.267 |
32 | 1'' | 2.9 | 0.259 | 3.6 | 0.313 | 4.4 | 0.371 | 5.4 | 0.436 |
40 | 1 1/4'' | 3.7 | 0.411 | 4.5 | 0.488 | 5.5 | 0.578 | 6.7 | 0.676 |
50 | 1 1/2'' | 4.6 | 0.631 | 5.6 | 0.75 | 6.9 | 0.894 | 8.3 | 1.041 |
63 | 2'' | 5.8 | 0.993 | 7.1 | 1.209 | 8.6 | 1.404 | 10.5 | 1.655 |
75 | 2 3/4'' | 6.8 | 1.377 | 8.4 | 1.679 | 10.3 | 2 | 12.5 | 2.345 |
90 | 3'' | 8.2 | 1.957 | 10.1 | 2.422 | 12.3 | 2.869 | 15 | 3.487 |
110 | 4'' | 10 | 3.013 | 12.3 | 3.61 | 15.1 | 4.301 | 18.3 | 5.037 |
160 | 6'' | 14.6 | 6.385 | 17.9 | 7.63 | 21.9 | 8.927 | 26.6 | 10.601 |
APPLICATION
1: Hot and cold potable water piping system in residential and commercial buildings,hospitals,hotels etc.
2: Food transportation
3: Industrial and medical fluids transportation
TEST & INSPECTION
TEST | REQUIREMENT | RESULT |
Visual Inspection | There is no color aberration for PPR pipe,PPR pipe surface must be smooth, without hollow,bubble,visible impurity or any other defect | Qualified |
Non-Transparency Test | PPR pipe shouldn't be transparent | Light Proof |
Vertical Reversion Rate | ≤2% | 0.7 |
Impact Test | damage rate | No damage |
Hydro-static Pressure Test | 1 6 Mpa pressure for 1 hour under 20℃ temperature | No crack,no leakage |
4.2 Mpa pressure for 22 hours under 95℃ temperature | No crack,no leakage | |
3.8 Mpa pressure for 165 hours under 95℃ temperature | No crack,no leakage | |
3.5 Mpa pressure for 1000 hours under 95℃ temperature | No crack,no leakage |
SOCKET FUSION JOINT FOR PPR PIPE SYSTEM
1 Fusion Preparation
Choose the suitable sockets and install, and prepare the fusion machine, tools, and fusion material
2 Cutting the PPR pipe
Cutting the requested length with the specified PPR pipe cutter
3 PPR pipe Cleaning
Cleaning the PPR pipe welding Surface with alcohol
4 Measure Depth
Marking the suitable depth for specified PPR pipe
5 Heating
Push the PPR pipe and PPR fitting into the welding tool up to the welding depth without turning
6 Fusion and Connecting
Push the heated pipe fitting exactly and suitable adjustments, adjustment should be finished within 5 seconds
The PPR Pipe Fusion Date Sheet
Diameter (mm) | Welding Depth (mm) | Heating Time (s) | Welding Time (s) | Cooling Time (min) |
20 | 14 | 5 | 4 | 2 |
25 | 15 | 7 | 4 | 2 |
32 | 16.5 | 8 | 6 | 4 |
40 | 18 | 12 | 6 | 4 |
50 | 20 | 18 | 6 | 4 |
63 | 24 | 24 | 8 | 6 |
75 | 26 | 30 | 8 | 8 |
90 | 29 | 40 | 8 | 8 |
110 | 32.5 | 50 | 10 | 8 |
Remarks :
→ The heating time for the PPR pipe should comply with the requirement of PPR products and be adjusted according to the working temperature.when the working temperature is bellow 5℃,the heating time should be extended by 50%.
→ When the heating was finished, quickly remove the pipe and fitting from the welding tools, join them immediately without turning until the marked welding depth is covered by the bead of PPR from the fittings
→ The joint elements have to be fixed during the specified assembly time, after the cooling period, the fusion joint is ready for use